Izici
1.Ukumelana namanzi okuhle kakhulu nokumelana nokugqwala.
I-2.Ukumelana okuhle kwamakhemikhali nokumelana nowoyela.
I-3.Ukunamathela okuhle, ukumelana nomthelela, ukumelana nokugqoka
Ukusetshenziswa okunconyiwe
Ukuze uthole ukuvikelwa kwensimbi nokhonkolo ezindaweni ezigqwala kakhulu, kungasetshenziswa njengejazi eliphakathi noma njengejazi eliphezulu lezakhiwo zangaphakathi.
Imiyalo yohlelo lokusebenza
Ukwelashwa kwe-substrate kanye ne-surface
Sifoni:ukuqhuma kuhlanzwe ku-Sa2.5 (ISO8501-1) noma ubuncane be-SSPC SP-6, iphrofayela eqhumayo i-Rz50μm~100μm (ISO8503-1) noma ithuluzi lamandla elihlanzwe ukuze libe ubuncane be-ISO-St3.0/SSPC SP3
Zonke izindawo ezigcotshwe kufanele zihlanzeke, zome futhi zingabi nokungcola, futhi kufanele zihlolwe futhi ziphathwe ngokuvumelana ne-ISO8504.
I-primer ye-workshop ehlanganiswe ngaphambili:Ukushisela, ukulinganisa iziqhumane kanye nomonakalo kufanele ukuqhuma kuhlanzwe ku-Sa2.5 (ISO8501-1), noma ithuluzi lamandla lihlanzwe ku-St3.0.
Thawu:Susa amafutha phezulu bese ususa usawoti nokunye ukungcola.
Cindawo engaphezulu:Ukufaka i-sealer efanelekile ukuvala izimbotshana ezingaphezulu ngaphambi kokufaka.
Oindawo yaso:sicela uthintane ne-ZINDN.
Kuyasebenza Futhi Ukwelapha
● Izinga lokushisa lendawo ezungezile kufanele libe ukusuka ku-5℃ ukuya ku-38℃, umswakama womoya ohlobene akufanele ube ngaphezu kwama-85%.
● Izinga lokushisa elingaphansi komhlaba ngesikhathi sokufakwa kanye nokwelapha kufanele libe ngu-3℃ ngaphezu kwendawo yamazolo.
● Ukusetshenziswa kwangaphandle akuvunyelwe esimweni sezulu esibi njengemvula, inkungu, iqhwa, umoya onamandla nothuli olunzima.
Impilo yebhodwe
5℃ | 15℃ | 25℃ | 35℃ |
4 amahora | 3 amahora | 2 amahora | 1.5 amahora |
Izindlela zokufaka isicelo
Isifutho esingenamoya, isifutho somoya asinconywa.
Ukugqoka ibhulashi ne-roller kunconywa kuphela ngejazi lemigqa, ukumbozwa kwendawo encane noma ukulungisa.
Imingcele yohlelo lokusebenza
Indlela yohlelo lokusebenza | Iyunithi | Isifutho esingenamoya | Ibhulashi/Irola |
I-Nozzle orifice | mm | 0.43-0.53 | —- |
Umfutho weNozzle | kg/cm2 | 150-200 | —- |
Mncane | % | 0~10 | 5; 10 |
Ukomisa & Ukwelapha
Indawo ye-substrate izinga lokushisa | 5℃ | 15℃ | 25℃ | 35℃ |
Ingaphezulu-yomile | 16 amahora. | 8 amahora. | 4 amahora. | 2 amahora. |
Ngomile | amahora 48. | Amahora angu-24. | 12 amahora. | 6 amahora. |
Ulapheke ngokugcwele | Izinsuku ezingu-14 | Izinsuku ezingu-10 | 6 izinsuku | 4 izinsuku |
Isikhathi sokuphumula sokuphumula (Okuncane) | amahora 48 | Amahora angu-24. | 12 amahora. | 6 amahora. |
Isikhathi sokuphumula sokuphumula (Ubuningi.) (usendlalelo esingu-no.2) | Izinsuku ezingu-14 | Izinsuku ezingu-10 | 6 izinsuku | 4 izinsuku |
Isikhathi sokuphumula sokuphumula (Ubuningi.) (Ijazi) | izinsuku ezingu-30 | izinsuku ezingu-20 | Izinsuku ezingu-14 | 7 izinsuku |
Ukwandulela & Okulandelayo
Ijazi elandulele:I-Epoxy zinc phosphate, i-Epoxy zinc ecebile, i-Epoxy primer, ingasetshenziswa futhi ngokuqondile ekuqhumeni kwensimbi okuhlanzwe ku-Sa2.5 (ISO8501-1).
Ijazi elilandelanayo:I-Epoxy topcoat, i-Polyurethane, i-Fluorocarbon, i-Polysiloxane...njll
Ukupakisha & Isitoreji
Ukupakisha:isisekelo 24kg, i-ejenti yokwelapha 4kg
Iphuzu elikhanyayo:>25℃(Ingxube)
Isitoreji:Kufanele igcinwe ngokuhambisana nemithetho kahulumeni wendawo.Indawo yokugcina impahla kufanele yomile, ipholile, ingene umoya futhi iqhelelane nokushisa nemithombo yomlilo.Isitsha sokupakisha kufanele sigcinwe sivalwe ngokuqinile.
Impilo yeshelufu:Unyaka ongu-1 ngaphansi kwezimo ezinhle zokugcina kusukela ngesikhathi sokukhiqiza.